Parts › 3D-print filaments › Bambu Lab ABS-GF
0 pickedCompare
Filament spool 1 kg (200 mm across, 65 mm wide)
ABS-GF: a picture of the part type, not this model. How it works

Bambu Lab ABS-GF

Bambu Lab ABS-GF: glass-fibre-filled ABS 3D-printer filament product line. Open Filament Database entry (MIT) with 8 colour variants, offered in 1.75 mm; gives density, nozzle and bed temperatures, drying settings, 16 data-sheet mechanical and thermal values.

Key specifications

Key specifications
Nozzle temperature240 to 280 °C source
Bed temperature80 to 100 °C source
Density1.08 g/cm³ source
Tensile strength36 MPa, 29 MPa 2 sources
Young's modulus3,160 MPa, 2,250 MPa 2 sources
Elongation at break6.3 %, 2.3 % 2 sources
Heat deflection temp.88 °C, 99 °C 2 sources

· Maker or source page

Specifications

Specifications
AttributeValueConditionsTypeSource, read date, quote
Nozzle temperature240 to 280 °Crecommended nozzle temperature range (OFD fields min_print_temperature to max_print_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1449 is consistent (250 °C)claimgithub.com 2026-11-16“"min_print_temperature": 240, "max_print_temperature": 280”
Bed temperature80 to 100 °Crecommended bed temperature range (OFD fields min_bed_temperature to max_bed_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1449 is consistent (90 °C)claimgithub.com 2026-11-16“"min_bed_temperature": 80, "max_bed_temperature": 100”
Density1.08 g/cm3OFD field density, g/cm³ per schemas/filament_schema.json; SpoolmanDB filaments/bambulab.json line 1449 gives the same densityclaimgithub.com 2026-11-16“"density": 1.08”
Tensile strength36 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "XY", "value": 36, "plus_minus": 3, "unit": "MPa"”
29 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "Z", "value": 29, "plus_minus": 3, "unit": "MPa"”
Young's modulus3160 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 170 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "XY", "value": 3160, "plus_minus": 170, "unit": "MPa"”
2250 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 130 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "Z", "value": 2250, "plus_minus": 130, "unit": "MPa"”
Elongation at break6.3 %XY print direction; ISO 527, GB/T 1040; plus or minus 1.2 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "XY", "value": 6.3, "plus_minus": 1.2, "unit": "%"”
2.3 %Z print direction; ISO 527, GB/T 1040; plus or minus 0.8 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "Z", "value": 2.3, "plus_minus": 0.8, "unit": "%"”
Heat deflection temp.99 °CHDT at 0.45 MPa load; ISO 75 0.45 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_045", "direction": "unknown", "value": 99, "unit": "°C"”
88 °CHDT at 1.8 MPa load; ISO 75 1.8 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_18", "direction": "unknown", "value": 88, "unit": "°C"”
Diameter tolerance0.03 mmplus or minus, on the filament diameter (OFD field diameter_tolerance, mm per schemas/filament_schema.json; 0.02 is the schema default and is not taken)claimgithub.com 2026-11-16“"diameter_tolerance": 0.03”
Drying temperature80 °Crecommended drying temperature (OFD field dry_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_temperature": 80”
Drying time8 hrecommended drying time at the drying temperature (OFD field dry_time, hours per schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_time": 8”
Filament diameter1.75 mmoffered filament diameter (sizes.json field diameter, mm per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"diameter": 1.75”
Flexural modulus2860 MPa = 2.86 GPaXY print direction; ISO 178, GB/T 9341; plus or minus 130 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "XY", "value": 2860, "plus_minus": 130, "unit": "MPa"”
1970 MPa = 1.97 GPaZ print direction; ISO 178, GB/T 9341; plus or minus 110 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "Z", "value": 1970, "plus_minus": 110, "unit": "MPa"”
Flexural strength68 MPaXY print direction; ISO 178, GB/T 9341; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "XY", "value": 68, "plus_minus": 4, "unit": "MPa"”
46 MPaZ print direction; ISO 178, GB/T 9341; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "Z", "value": 46, "plus_minus": 3, "unit": "MPa"”
Impact strength14.5 kJ/m2XY print direction; ISO 179, GB/T 1043; plus or minus 1.5 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "XY", "value": 14.5, "plus_minus": 1.5, "unit": "kJ/m2"”
5.3 kJ/m2Z print direction; ISO 179, GB/T 1043; plus or minus 1.4 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "Z", "value": 5.3, "plus_minus": 1.4, "unit": "kJ/m2"”
Impact strength notched4.2 kJ/m2notched; XY print direction; ISO 179, GB/T 1043; plus or minus 1.1 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength_notched", "direction": "XY", "value": 4.2, "plus_minus": 1.1, "unit": "kJ/m2"”
Spool net mass1000 g = 1 kgoffered net filament weight per spool (sizes.json field filament_weight, grams per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"filament_weight": 1000”
Vicat softening temperature103 °CISO 306, GB/T 1633; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/69f0758087c943f8a0a87bffa6dc901b.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "vicat_softening", "direction": "unknown", "value": 103, "unit": "°C"”

Variations from this maker

ABS