Parts › 3D-print filaments › Bambu Lab ASA
0 pickedCompare
Filament spool 1 kg, ASA; the spool colour marks the family, it is not a property of the material
ASA: a picture of the part type, not this model. How it works

Bambu Lab ASA

Bambu Lab ASA: ASA 3D-printer filament product line. Open Filament Database entry (MIT) with 7 colour variants, offered in 1.75 mm; gives density, nozzle and bed temperatures, drying settings, 16 data-sheet mechanical and thermal values.

Key specifications

Key specifications
Nozzle temperature240 to 270 °C source
Bed temperature80 to 100 °C source
Density1.05 g/cm³ source
Tensile strength37 MPa, 31 MPa 2 sources
Young's modulus2,450 MPa, 2,120 MPa 2 sources
Elongation at break9.2 %, 4.6 % 2 sources
Heat deflection temp.92 °C, 100 °C 2 sources

· Maker or source page

Specifications

Specifications
AttributeValueConditionsTypeSource, read date, quote
Nozzle temperature240 to 270 °Crecommended nozzle temperature range (OFD fields min_print_temperature to max_print_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"min_print_temperature": 240, "max_print_temperature": 270”
Bed temperature80 to 100 °Crecommended bed temperature range (OFD fields min_bed_temperature to max_bed_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"min_bed_temperature": 80, "max_bed_temperature": 100”
Density1.05 g/cm3OFD field density, g/cm³ per schemas/filament_schema.jsonclaimgithub.com 2026-11-16“"density": 1.05”
Tensile strength37 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "XY", "value": 37, "plus_minus": 3, "unit": "MPa"”
31 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "Z", "value": 31, "plus_minus": 4, "unit": "MPa"”
Young's modulus2450 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 270 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "XY", "value": 2450, "plus_minus": 270, "unit": "MPa"”
2120 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 260 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "Z", "value": 2120, "plus_minus": 260, "unit": "MPa"”
Elongation at break9.2 %XY print direction; ISO 527, GB/T 1040; plus or minus 1.4 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "XY", "value": 9.2, "plus_minus": 1.4, "unit": "%"”
4.6 %Z print direction; ISO 527, GB/T 1040; plus or minus 0.8 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "Z", "value": 4.6, "plus_minus": 0.8, "unit": "%"”
Heat deflection temp.100 °CHDT at 0.45 MPa load; ISO 75 0.45 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_045", "direction": "unknown", "value": 100, "unit": "°C"”
92 °CHDT at 1.8 MPa load; ISO 75 1.8 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_18", "direction": "unknown", "value": 92, "unit": "°C"”
Diameter tolerance0.03 mmplus or minus, on the filament diameter (OFD field diameter_tolerance, mm per schemas/filament_schema.json; 0.02 is the schema default and is not taken)claimgithub.com 2026-11-16“"diameter_tolerance": 0.03”
Drying temperature80 °Crecommended drying temperature (OFD field dry_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_temperature": 80”
Drying time8 hrecommended drying time at the drying temperature (OFD field dry_time, hours per schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_time": 8”
Filament diameter1.75 mmoffered filament diameter (sizes.json field diameter, mm per schemas/sizes_schema.json); first seen in colour variant aero_whiteclaimgithub.com 2026-11-16“"diameter": 1.75”
Flexural modulus1920 MPa = 1.92 GPaXY print direction; ISO 178, GB/T 9341; plus or minus 130 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "XY", "value": 1920, "plus_minus": 130, "unit": "MPa"”
1650 MPa = 1.65 GPaZ print direction; ISO 178, GB/T 9341; plus or minus 120 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "Z", "value": 1650, "plus_minus": 120, "unit": "MPa"”
Flexural strength65 MPaXY print direction; ISO 178, GB/T 9341; plus or minus 5 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "XY", "value": 65, "plus_minus": 5, "unit": "MPa"”
40 MPaZ print direction; ISO 178, GB/T 9341; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "Z", "value": 40, "plus_minus": 3, "unit": "MPa"”
Impact strength41.0 kJ/m2XY print direction; ISO 179, GB/T 1043; plus or minus 2.3 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "XY", "value": 41.0, "plus_minus": 2.3, "unit": "kJ/m2"”
4.9 kJ/m2Z print direction; ISO 179, GB/T 1043; plus or minus 0.6 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "Z", "value": 4.9, "plus_minus": 0.6, "unit": "kJ/m2"”
Impact strength notched19.6 kJ/m2notched; XY print direction; ISO 179, GB/T 1043; plus or minus 1.8 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength_notched", "direction": "XY", "value": 19.6, "plus_minus": 1.8, "unit": "kJ/m2"”
Spool net mass1000 g = 1 kgoffered net filament weight per spool (sizes.json field filament_weight, grams per schemas/sizes_schema.json); first seen in colour variant aero_whiteclaimgithub.com 2026-11-16“"filament_weight": 1000”
Vicat softening temperature106 °CISO 306, GB/T 1633; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/ad7b08230c164e72856cffbe06bb7dc9.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "vicat_softening", "direction": "unknown", "value": 106, "unit": "°C"”

Variations from this maker

ASA Aero · ASA-CF