Parts › 3D-print filaments › Bambu Lab PETG-CF
0 pickedCompare
Filament spool 1 kg, PETG with carbon fibre (near black); the label colour marks the family, it is not a property of the material
PETG-CF: a picture of the part type, not this model. How it works

Bambu Lab PETG-CF

Bambu Lab PETG-CF: carbon-fibre-filled PETG 3D-printer filament product line. Open Filament Database entry (MIT) with 6 colour variants, offered in 1.75 mm; gives density, nozzle and bed temperatures, drying settings, 16 data-sheet mechanical and thermal values.

Key specifications

Key specifications
Nozzle temperature240 to 270 °C source
Bed temperature65 to 75 °C source
Density1.25 g/cm³ source
Tensile strength35 MPa, 29 MPa 2 sources
Young's modulus2,460 MPa, 1,340 MPa 2 sources
Elongation at break10.4 %, 4.7 % 2 sources
Heat deflection temp.68 °C, 74 °C 2 sources

· Maker or source page

Specifications

Specifications
AttributeValueConditionsTypeSource, read date, quote
Nozzle temperature240 to 270 °Crecommended nozzle temperature range (OFD fields min_print_temperature to max_print_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1985 is consistent (270 °C)claimgithub.com 2026-11-16“"min_print_temperature": 240, "max_print_temperature": 270”
Bed temperature65 to 75 °Crecommended bed temperature range (OFD fields min_bed_temperature to max_bed_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1985 is consistent (75 °C)claimgithub.com 2026-11-16“"min_bed_temperature": 65, "max_bed_temperature": 75”
Density1.25 g/cm3OFD field density, g/cm³ per schemas/filament_schema.json; SpoolmanDB filaments/bambulab.json line 1985 gives the same densityclaimgithub.com 2026-11-16“"density": 1.25”
Tensile strength35 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 5 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "XY", "value": 35, "plus_minus": 5, "unit": "MPa"”
29 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "Z", "value": 29, "plus_minus": 4, "unit": "MPa"”
Young's modulus2460 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 230 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "XY", "value": 2460, "plus_minus": 230, "unit": "MPa"”
1340 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 150 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "Z", "value": 1340, "plus_minus": 150, "unit": "MPa"”
Elongation at break10.4 %XY print direction; ISO 527, GB/T 1040; plus or minus 0.6 %; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "XY", "value": 10.4, "plus_minus": 0.6, "unit": "%"”
4.7 %Z print direction; ISO 527, GB/T 1040; plus or minus 0.4 %; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "Z", "value": 4.7, "plus_minus": 0.4, "unit": "%"”
Heat deflection temp.74 °CHDT at 0.45 MPa load; ISO 75 0.45 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_045", "direction": "unknown", "value": 74, "unit": "°C"”
68 °CHDT at 1.8 MPa load; ISO 75 1.8 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_18", "direction": "unknown", "value": 68, "unit": "°C"”
Diameter tolerance0.03 mmplus or minus, on the filament diameter (OFD field diameter_tolerance, mm per schemas/filament_schema.json; 0.02 is the schema default and is not taken)claimgithub.com 2026-11-16“"diameter_tolerance": 0.03”
Drying temperature65 °Crecommended drying temperature (OFD field dry_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_temperature": 65”
Drying time8 hrecommended drying time at the drying temperature (OFD field dry_time, hours per schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_time": 8”
Filament diameter1.75 mmoffered filament diameter (sizes.json field diameter, mm per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"diameter": 1.75”
Flexural modulus2910 MPa = 2.91 GPaXY print direction; ISO 178, GB/T 9341; plus or minus 260 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "XY", "value": 2910, "plus_minus": 260, "unit": "MPa"”
1560 MPa = 1.56 GPaZ print direction; ISO 178, GB/T 9341; plus or minus 180 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "Z", "value": 1560, "plus_minus": 180, "unit": "MPa"”
Flexural strength70 MPaXY print direction; ISO 178, GB/T 9341; plus or minus 5 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "XY", "value": 70, "plus_minus": 5, "unit": "MPa"”
48 MPaZ print direction; ISO 178, GB/T 9341; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "Z", "value": 48, "plus_minus": 4, "unit": "MPa"”
Impact strength41.2 kJ/m2XY print direction; ISO 179, GB/T 1043; plus or minus 2.6 kJ/m2; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "XY", "value": 41.2, "plus_minus": 2.6, "unit": "kJ/m2"”
10.7 kJ/m2Z print direction; ISO 179, GB/T 1043; plus or minus 1.6 kJ/m2; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "Z", "value": 10.7, "plus_minus": 1.6, "unit": "kJ/m2"”
Impact strength notched15.7 kJ/m2notched; XY print direction; ISO 179, GB/T 1043; plus or minus 1.6 kJ/m2; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength_notched", "direction": "XY", "value": 15.7, "plus_minus": 1.6, "unit": "kJ/m2"”
Spool net mass1000 g = 1 kgoffered net filament weight per spool (sizes.json field filament_weight, grams per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"filament_weight": 1000”
Vicat softening temperature85 °CISO 306, GB/T 1633; printed specimen, 100% infill; annealed and dried at 65 °C for 8 h; from the brand's data sheet https://store.bblcdn.com/626e4f424bf345ae965ad0ddfcaf2459.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "vicat_softening", "direction": "unknown", "value": 85, "unit": "°C"”

Variations from this maker

PETG HF · PETG Basic · PETG Matte · PETG Translucent