Bambu Lab PC FR

Bambu Lab PC FR: PC 3D-printer filament product line. Open Filament Database entry (MIT) with 3 colour variants, offered in 1.75 mm; gives density, nozzle and bed temperatures, drying settings, 16 data-sheet mechanical and thermal values.

Key specifications

Key specifications
Nozzle temperature260 to 280 °C source
Bed temperature90 to 110 °C source
Density1.18 g/cm³, 1.19 g/cm³ 2 sources
Tensile strength60 MPa, 21 MPa 2 sources
Young's modulus1,670 MPa, 1,450 MPa 2 sources
Elongation at break2.4 %, 1.5 % 2 sources
Heat deflection temp.108 °C, 113 °C 2 sources

· Maker or source page

Specifications

Specifications
AttributeValueConditionsTypeSource, read date, quote
Nozzle temperature260 to 280 °Crecommended nozzle temperature range (OFD fields min_print_temperature to max_print_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1597 is consistent (270 °C)claimgithub.com 2026-11-16“"min_print_temperature": 260, "max_print_temperature": 280”
Bed temperature90 to 110 °Crecommended bed temperature range (OFD fields min_bed_temperature to max_bed_temperature; unit per OFD schemas/filament_schema.json); SpoolmanDB filaments/bambulab.json line 1597 is consistent (110 °C)claimgithub.com 2026-11-16“"min_bed_temperature": 90, "max_bed_temperature": 110”
Density1.18 g/cm3OFD field density, g/cm³ per schemas/filament_schema.jsonclaimgithub.com 2026-11-16“"density": 1.18”
1.19 g/cm3SpoolmanDB filaments/bambulab.json, object 'FR {color_name}' (PC); kept beside the Open Filament Database value because they differ or the OFD entry lacks it; g/cm3 per SpoolmanDB README.mdclaimgithub.com 2026-11-16“"density": 1.19”
Tensile strength60 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "XY", "value": 60, "plus_minus": 4, "unit": "MPa"”
21 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 3 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_strength", "direction": "Z", "value": 21, "plus_minus": 3, "unit": "MPa"”
Young's modulus1670 MPaXY print direction; ISO 527, GB/T 1040; plus or minus 40 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "XY", "value": 1670, "plus_minus": 40, "unit": "MPa"”
1450 MPaZ print direction; ISO 527, GB/T 1040; plus or minus 60 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "tensile_modulus", "direction": "Z", "value": 1450, "plus_minus": 60, "unit": "MPa"”
Elongation at break2.4 %XY print direction; ISO 527, GB/T 1040; plus or minus 0.3 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "XY", "value": 2.4, "plus_minus": 0.3, "unit": "%"”
1.5 %Z print direction; ISO 527, GB/T 1040; plus or minus 0.4 %; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "elongation_at_break", "direction": "Z", "value": 1.5, "plus_minus": 0.4, "unit": "%"”
Heat deflection temp.113 °CHDT at 0.45 MPa load; ISO 75 0.45 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_045", "direction": "unknown", "value": 113, "unit": "°C"”
108 °CHDT at 1.8 MPa load; ISO 75 1.8 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "heat_deflection_18", "direction": "unknown", "value": 108, "unit": "°C"”
Diameter tolerance0.03 mmplus or minus, on the filament diameter (OFD field diameter_tolerance, mm per schemas/filament_schema.json; 0.02 is the schema default and is not taken)claimgithub.com 2026-11-16“"diameter_tolerance": 0.03”
Drying temperature80 °Crecommended drying temperature (OFD field dry_temperature; unit per OFD schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_temperature": 80”
Drying time8 hrecommended drying time at the drying temperature (OFD field dry_time, hours per schemas/filament_schema.json)claimgithub.com 2026-11-16“"dry_time": 8”
Filament diameter1.75 mmoffered filament diameter (sizes.json field diameter, mm per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"diameter": 1.75”
Flexural modulus1890 MPa = 1.89 GPaXY print direction; ISO 178, GB/T 9341; plus or minus 70 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "XY", "value": 1890, "plus_minus": 70, "unit": "MPa"”
1660 MPa = 1.66 GPaZ print direction; ISO 178, GB/T 9341; plus or minus 80 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_modulus", "direction": "Z", "value": 1660, "plus_minus": 80, "unit": "MPa"”
Flexural strength90 MPaXY print direction; ISO 178, GB/T 9341; plus or minus 4 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "XY", "value": 90, "plus_minus": 4, "unit": "MPa"”
47 MPaZ print direction; ISO 178, GB/T 9341; plus or minus 2 MPa; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "flexural_strength", "direction": "Z", "value": 47, "plus_minus": 2, "unit": "MPa"”
Impact strength55 kJ/m2XY print direction; ISO 179, GB/T 1043; plus or minus 2.1 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "XY", "value": 55, "plus_minus": 2.1, "unit": "kJ/m2"”
8.0 kJ/m2Z print direction; ISO 179, GB/T 1043; plus or minus 0.4 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength", "direction": "Z", "value": 8.0, "plus_minus": 0.4, "unit": "kJ/m2"”
Impact strength notched8.4 kJ/m2notched; XY print direction; ISO 179, GB/T 1043; plus or minus 1.3 kJ/m2; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "impact_strength_notched", "direction": "XY", "value": 8.4, "plus_minus": 1.3, "unit": "kJ/m2"”
Spool net mass1000 g = 1 kgoffered net filament weight per spool (sizes.json field filament_weight, grams per schemas/sizes_schema.json); first seen in colour variant blackclaimgithub.com 2026-11-16“"filament_weight": 1000”
Vicat softening temperature114 °CISO 306, GB/T 1633; printed specimen, 100% infill; annealed and dried at 80 °C for 12 h; from the brand's data sheet https://store.bblcdn.com/s1/default/4adf3c9827a0475d8777e9b8cfd11fbe.pdf (primary source, read by OFD contributors 2026-11-08)specgithub.com 2026-11-16“"property": "vicat_softening", "direction": "unknown", "value": 114, "unit": "°C"”

Variations from this maker

PC