Generic Steel 4140 (quenched and tempered)
AISI/SAE 4140 chromium-molybdenum steel in the quenched and tempered state, a common grade for shafts, gears and highly loaded pins; strength falls as the section grows, so the values are given per diameter band.
Key specifications
| Yield strength | 900 MPa, 750 MPa, 650 MPa, 550 MPa and more source |
|---|---|
| Tensile strength | 1,100 to 1,300 MPa, 1,000 to 1,200 MPa, 900 to 1,100 MPa, 800 to 950 MPa and more source |
Specifications
| Attribute | Value | Conditions | Type | Source, read date, quote |
|---|---|---|---|---|
| Yield strength | 550 MPa | minimum, quenched and tempered, 100 < d ≤ 160 mm (60 < t ≤ 100 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“80 ksi (550 MPa)” |
| 750 MPa | minimum, quenched and tempered, 16 < d ≤ 40 mm (8 < t ≤ 20 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“109 ksi (750 MPa)” | |
| 500 MPa | minimum, quenched and tempered, 160 < d ≤ 250 mm (100 < t ≤ 160 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“73 ksi (500 MPa)” | |
| 650 MPa | minimum, quenched and tempered, 40 < d ≤ 100 mm (20 < t ≤ 60 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“94 ksi (650 MPa)” | |
| 900 MPa | minimum, quenched and tempered, d ≤ 16 mm (t ≤ 8 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“Yield Strength (Min) 130 ksi (900 MPa)” | |
| Tensile strength | 800 to 950 MPa | quenched and tempered, 100 < d ≤ 160 mm (60 < t ≤ 100 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“116–138 ksi (800–950 MPa)” |
| 1000 to 1200 MPa | quenched and tempered, 16 < d ≤ 40 mm (8 < t ≤ 20 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“150–170 ksi (1,000–1,200 MPa)” | |
| 750 to 900 MPa | quenched and tempered, 160 < d ≤ 250 mm (100 < t ≤ 160 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“109–131 ksi (750–900 MPa)” | |
| 900 to 1100 MPa | quenched and tempered, 40 < d ≤ 100 mm (20 < t ≤ 60 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“130–160 ksi (900–1,100 MPa)” | |
| 1100 to 1300 MPa | quenched and tempered, section diameter d ≤ 16 mm (thickness t ≤ 8 mm); table cites [4]; Wikipedia article 41xx steel, revision 1382900922 | claim | en.wikipedia.org 2026-11-16“Tensile Strength 160–190 ksi (1,100–1,300 MPa)” |